A polyaryletherketone polymeric material, for example polyetheretherketone
and composite materials comprising said polymeric material are described.
The polymeric material has a melt viscosity (MV) in the range 0.05 to
0.12 kNsm.sup.-2, preferably in the range 0.085 to 0.095 kNsm.sup.-2.