A method of making an ink-printed fibrous web by applying onto at least one side of a coated fibrous web at least one ink layer of a planographic ink to form an image thereon to produce a printed fibrous web. The ink layer(s) has a total volatile content, as supplied, of less than 10% (preferably less than 5%). The printed fibrous web is then subjected to ambient temperatures without the use of a drying oven or by employing oven temperatures that have an exit web temperature that does not exceed 225.degree. F. Subsequent processing of the printed fibrous web includes applying one or more coatings including a waterbased coating, a coating having a total volatile content of less than 10%, a coating that is cured with actinic radiation, and an anti-offset coating.

 