Disclosed herein is a refinish sheet produced by (1) coating one side of a temporary carrier sheet (A) with at least one aqueous coating material (B) comprising at least one free-radically crosslinkable binder (B1) having a glass transition temperature of -70 to +50.degree. C., an olefinically unsaturated double bond content of 2 to 10 eq/kg, and an acid group content of 0.05 to 15 eq/kg to produce at least one resultant layer (B); and (2) drying but not curing, or only part-curing, the at least one resultant layer (B) to produce at least one dried, uncured or part-cured layer (B). Also disclosed is a method of repairing a surface of a coated substrate using the refinish sheet.

 