A heap is constructed with hypogenic copper sulfide bearing ore to include exposed sulfide mineral particles at least 25 weight % of which are hypogenic copper sulfides. The concentration of the exposed sulfide mineral particles is such that the heap includes at least 10 Kg of exposed sulfide sulfur per tonne of solids in the heap. At least 50% of the total copper in the heap is in the form of hypogenic copper sulfides. A substantial portion of the heap is heated to at least 50.degree. C. The heap is inoculated with a thermophilic microorganism, and bioleaching is carried out so that sufficient sulfide mineral particles in the heap are biooxidized to oxidize at least 10 Kg of sulfide sulfur per tonne of solids in the heap and to cause the dissolution of at least 50% of the copper in the heap in a relatively short period of time.

 