A method of fabricating a semiconductor device having a silicon nitride layer substantially free of impurities includes forming a silicon nitride layer on a semiconductor substrate and annealing the semiconductor substrate having the silicon nitride layer in an atmosphere of ammonia (NH.sub.3) gas to remove impurities from the silicon nitride layer. The silicon nitride layer may be formed using BTBAS as a silicon precursor.

 