The rear projection screen includes a laminated sheet having a multi-layered structure consisting of the n number (n is a natural number of three or above) of layers. In this laminated sheet, a difference in linear expansion coefficients is 5% or more between a layer having the maximum linear expansion coefficient and a layer having the minimum linear expansion coefficient. Further, a difference in elasticity is 10% or more between a layer having the maximum elasticity and a layer having the minimum elasticity. The curvature change rate .epsilon. (1/mm.degree. C.) of the laminated sheet with respect to temperature satisfies -7.0.times.10.sup.-6.ltoreq..epsilon..ltoreq.7.0.times.10.sup.-6.

 