The present invention provides non-axially symmetrical manufactured parts of thickness less than 10 mm, made of or quasi- titanium alloy, having a core microstructure constituted by whole grains presenting a slenderness ratio greater than 4 and an equivalent diameter lying in the range 10 m to 300 m. The invention also provides a method of manufacturing the parts by forging.

 