A negative electrode of a nonaqueous secondary battery is formed of a carbonaceous material. The ratio RG=Gs/Gb of the degree of graphitization Gs of the carbonaceous material, determined by a surface-enhanced Raman spectrum, to the degree of graphitization Gb, determined by a Raman spectrum measured using argon laser light, is at least 4.5. Alternatively, the carbonaceous material has a peak in a wavelength range above 1,360 cm-1 in a surface-enhanced Raman spectrum which is measured by the same surface-enhanced Raman spectrum. The deterioration of the nonaqueous secondary battery is suppressed during use in high-temperature environments and high capacity is maintained for long periods.

 
Web www.patentalert.com

< Steam methane reforming method

< Carbonaceous material for hydrogen storage and method for preparation thereof, carbonaceous material having hydrogen absorbed therein and method for preparation thereof, cell and fuel cell using carbonaceous material having hydrogen absorbed therein

> Modified titanium dioxide and a method for its preparation

> Synthesis of metal compounds under carbothermal conditions

~ 00258