Actuator molding and baking process parameters for polyphenylene sulfide 40% glass fill for high temperature overmold carriage operation in hard disk drives

   
   

A method is provided for forming a body for a hard disk carriage assembly from polyphenylene sulfide 40% glass fill. An injection mold is heated to approximately 130.degree. C.; then a volume of polyphenylene sulfide 40% glass fill is injected into the mold to form the body of the carriage assembly. The polyphenylene sulfide 40% glass fill is then cooled within the mold for approximately 45 seconds before the body is ejected from the mold cavity. The body is then heated to approximately 130.degree. C. for at least 2 hours in a post-bake operation.

Un metodo è fornito per formare un corpo per un complessivo del carrello del disco rigido dal materiale di riempimento di vetro del solfuro 40% del polifenilene. Una muffa dell'iniezione è riscaldata ad approssimativamente 130.degree. C.; allora un volume del materiale di riempimento di vetro del solfuro 40% del polifenilene è iniettato nella muffa per formare il corpo del complessivo del carrello. Il materiale di riempimento di vetro del solfuro 40% del polifenilene allora è raffreddato all'interno della muffa per circa 45 secondi prima che il corpo sia espulso dalla cavità della muffa. Il corpo allora è riscaldato ad approssimativamente 130.degree. C. per almeno 2 ore in un funzionamento di alberino-cuoc.

 
Web www.patentalert.com

< Disc head slider designs with particle flushing channels

< Electrical interconnect scheme

> Remote-operated integrated microactuator, in particular for a read/write transducer of hard disks

> Light induction type thin film magnetic head

~ 00140