Disclosed herein is an elastomeric composition comprising propylene, the composition further comprising a peak melting point temperature below about 110.degree. C., a tensile set of 40% or less, and greater than or equal to about 60% [r]dyads, based on the total number of dyads present in the composition. A process to produce an elastomeric composition is also disclosed.

 