The invention relates to a method for regenerating denox catalysts having an increased SO.sub.2/SO.sub.3 conversion rate as a result of the cumulation of iron compounds, and is characterized in that the catalysts are treated with an essentially aqueous acid solution, preferably having a pH between 0.5 and 4, and with an addition of antioxidants.

 
Web www.patentalert.com

< Enhanced Thickness Fabric and Method of Making Same

> Fire retardant foam and methods of use

> MODIFIERS FOR GYPSUM SLURRIES AND METHOD OF USING THEM

~ 00561