The present invention provides high density cobalt-manganese coprecipitated nickel hydroxide, particularly having a tapping density of 1.5 g/cc or greater, and a process for its production characterized by continuous supply of an aqueous solution of a nickel salt which contains a cobalt salt and a manganese salt, of a complexing agent and of an alkali metal hydroxide, into a reactor either in an inert gas atmosphere or in the presence of a reducing agent, continuous crystal growth and continuous removal.

 