A polarizing plate having excellent moisture durability and a liquid crystal display using the same are disclosed. The polarizing plate is produced by covering all surfaces and sides of a polarizer with low moisture-permeable layers having moisture permeability of 310 g/m224 h or less. The rate of change in dimension of the polarizer in the uniaxially stretched direction is 0.1% or less after left at a temperature of 60 C. and humidity of 95% for 100 hours.

 