Microwave assisted continuous synthesis of nanocrystalline powders and coatings using the polyol process

   
   

A method of forming a nanocrystalline metal, comprising the steps of: providing a reaction mixture comprising a metal precursor and an alcohol solvent; continuously flowing the reaction mixture through a reactor; applying microwave or millimeter-wave energy to the reaction mixture; wherein the microwave or millimeter-wave energy is localized to the vicinity of the reaction mixture; and heating the reaction mixture with the microwave or millimeter-wave energy so that the alcohol solvent reduces the metal precursor to a metal; wherein the heating occurs in the reactor.

Un método de formar un metal del nanocrystalline, abarcando los pasos de: abastecimiento de una mezcla de reacción que abarca un precursor del metal y un solvente del alcohol; continuamente fluyendo la mezcla de reacción a través de un reactor; aplicación de microonda o de energía de la onda milimétrica a la mezcla de reacción; en donde la microonda o la energía de la onda milimétrica se localiza a la vecindad de la mezcla de reacción; y calefacción la mezcla de reacción con la microonda o la energía de la onda milimétrica de modo que el solvente del alcohol reduzca el precursor del metal a un metal; en donde la calefacción ocurre en el reactor.

 
Web www.patentalert.com

< Methods and compositions for inhibiting angiogenesis

< Silicon nanoparticle and method for producing the same

> Method of coating a luminescent material

> Mineral-filled coatings having enhanced abrasion resistance and wear clarity and methods for using the same

~ 00151