A method for producing an improved coextruded polymeric film is disclosed. First, a base layer containing a polymeric matrix and at least one additional layer on at least one side of the base layer are coextruded. If the coextruded polymeric film is to be opaque, the base layer also contains at least one cavitating agent. Next, the coextruded multi-layer film is cooled. Finally, the coextruded multi-layer film is oriented in at least the machine direction (MD). At least the base layer of the coextruded polymeric film contains a fluoropolymer. The inclusion of the fluoropolymer in at least the base layer of the coextruded polymeric film provides a more even distribution of polymer flow through a die, which in turns leads to improved film gauge uniformity.

Un método para producir mejorado coextruded la película polimérica se divulga. Primero, una capa baja que contiene una matriz polimérica y por lo menos una capa adicional en por lo menos un lado de la capa baja son coextruded. Si coextruded la película polimérica debe ser opaca, la capa baja también contiene por lo menos un agente de cavitación. Después, coextruded la película de múltiples capas se refresca. Finalmente, coextruded la película de múltiples capas se orienta en por lo menos la dirección de la máquina (MD). Por lo menos la capa baja de coextruded la película polimérica contiene un fluoropolymer. La inclusión del fluoropolymer en por lo menos la capa baja de coextruded la película polimérica proporciona una distribución más uniforme del polímero atraviesa un dado, que en vueltas conduce a la uniformidad mejorada de la galga de la película.

 
Web www.patentalert.com

< (none)

< Method for installation of evacuated tubular conduits

> High-pressure separation of a multi-component gas

> (none)

~ 00088