A porous glass rod is treated to include tungsten oxide and palladium in an arrangement that is sensitive to hydrogen to produce a color change that is a function of the hydrogen concentration. The rod is attached to the tip of a double fiber into one of which light is launched by a light source. A detector at the end of the second fiber is responsive to light reflected by the rod. The process for forming the rod includes the steps of doping the glass with a tungsten compound and a palladium compound with intervening and subsequent heating steps to bond the tungsten oxide and palladium to available oxygen atoms of the porous glass.

Una barra del cristal poroso se trata para incluir el óxido y el paladio del tungsteno en un arreglo que sea sensible al hidrógeno al producto al cambio del color que es una función de la concentración del hidrógeno. La barra se une a la extremidad de una fibra doble en una de el cual la luz sea lanzada por una fuente de luz. Un detector en el extremo de la segunda fibra es responsivo a la luz reflejada por la barra. El proceso para formar la barra incluye los pasos de dopar el cristal con un compuesto del tungsteno y un compuesto del paladio con pasos de la calefacción que intervienen y subsecuentes para enlazar el óxido y el paladio del tungsteno a los átomos de oxígeno disponibles del cristal poroso.

 
Web www.patentalert.com

< Electrochromic mirror

< Methods of preventing reduction of irox during PZT formation by metalorganic chemical vapor deposition or other processing

> Protection of tungsten alignment mark for FeRAM processing

> Perovskite-containing composite material, method of manufacturing said material, electronic component and module

~ 00064