Disclosed is a method of making an optical fiber preform having at least one annular region of depressed refractive index. A tube of silica doped with fluorine and/or boron is overclad with silica soot. A core rod is inserted into the overclad tube and the resultant assembly is heated while chlorine flows between the tube and the core rod to clean the adjacent surfaces. When the soot sinters, the tube collapses onto and fuses to the rod. The resultant tubular structure is formed into an optical fiber which exhibits low attenuation as a result of the low seed count at the interface between the inner core and the region that is doped with florine and/or boron.

Показан метод делать preform оптически волокна имея по крайней мере одну кольцевую зону отжатого рефрактивного индекса. Пробка кремнезема дала допинг с фтором and/or бор будет overclad с сажей кремнезема. Штанга сердечника введена в пробку overclad и возникающий агрегат нагрет пока хлор пропускает между пробкой и штангой сердечника для того чтобы очистить смежные поверхности. Когда сажа спекает, пробка рушится на и сплавляется к штанге. Возникающая трубчатая структура сформирована в оптически волокно exhibits низкая амортизация в результате низкого отсчета семени на поверхности стыка между внутренним сердечником и зоной дана допинг с florine and/or бором.

 
Web www.patentalert.com

< Fluorinating an optical fiber preform in a pure aluminum oxide muffle tube

< Fiber preform method with a hot drill-in step for a Ge-doped tube and an F-doped rod

> Method of purifying natural or synthetic silica, and application thereof to depositing purified natural or synthetic silica on an optical fiber preform

> Dispersion compensating fiber

~ 00039